Step 1

Area to be repaired.

Step 2

Infrared heating unit is lowered to within 6″ of the pavement.

Step 3

Having heated the area to be repaired, the softened asphalt is raked and cleared of impurities.

Step 4

New asphalt is stored at 300° and added to the repair area.

Step 5

New and original asphalt is blended and raked level.

Step 6

The edges are first rolled to bond the new asphalt with the original asphalt. The entire area is then compacted with a vibratory roller.

Step 7

The repair becomes a seamless part of the original asphalt.
Patch is completed in approximately 15 minutes.